Inkjet Printing on NanoPaper: Waveforms & Platen Temperature
*Applies to: A4 Sheets · Last updated: 2025-11-27 13:17:50*
Baseline setup
-
Platen: start 30–45 °C; increase for faster dry if edges remain crisp.
-
Waveform: vendor-recommended for your ink head; purge/prime before runs.
-
Drop spacing: start with vendor default; tighten only after adhesion validated.
Artifact control
-
Coffee-ring: increase platen temp or adjust solids; lengthen dwell between passes.
-
Satellites: tweak waveform/voltage; verify nozzle health.
-
Bleed: reduce ink laydown, lower platen temp, or increase inter-pass delay.
Post-process
-
Stepwise dry → anneal → sinter per ink. Verify solvent is fully removed before high-temp steps.
Metrology
-
Inspect edge roughness and minimum printable line.
-
Measure resistance of printed traces; track across print/cure iterations.